Current > Home > Cases > Power plant
Place of use:
Flue of desulfurization system in power plant.
Medium: flue gas containing sulfur dioxide and sulfur trioxide.
Temperature: low temperature part 60 ~ 100 ℃, high temperature part 100 ~ 150 ℃
Materials used:
Primer: Swancor 984-M (low temperature) Swancor 917 (high temperature)
Low temperature scale: Swancor 901-FLS
High temperature scale: Swancor 907-FLS
Top coat: Swancor 901 - FLSPW (low temperature) Swancor 907-FLSPW (high temperature)
Production method:
1. The surface of carbon steel is sandblasted to Sa21 / 2, and then roll coated with Swancor 984-M (or Swancor 917) primer.
2. Apply 2-3 layers of Swancor 901-FLS (or Swancor 907-FLS) with airless spraying equipment.
3. Spray one coat of Swancor 901-FLSPW (or Swancor 907-FLSPW) flake coating.
4. Through appearance, styrene sensitivity test, EDM and thickness detection.
- Power plant
- Wind blade
- Steel plant
- Copper smelting
- Other non-ferrous metal industry
- Chlor alkali chemical industry
- Treatment of waste water and waste gas
- Semiconductor electronics factory
- Electroplating & electrophoresis
- Pulp plant
- Fertilizer plant
- Seawater desalination
- Food & pharmaceutical industry
- Petrochemical Industry
- Ship application
- SMC/BMC
Cases